Nanoindentation is a sophisticated technique used to measure the mechanical properties of materials at the micro- to nano-scale. It works by pressing a sharp indenter tip into the surface of a material with controlled force and measuring the material's response to this deformation. The resulting data provides insights into properties such as hardness, elastic modulus, and creep behavior.
At Nano-characterisation Laboratory, we are equipped with the NanoTest Vantage and Hysitron TI Premier systems, two of the most advanced nanoindentation instruments available. Besides offering standard indentation and creep testing with ease, the NanoTest Vantage excels in conducting impact and scratch tests. It also includes modules for liquid and high-temperature testing. On the other hand, the TI Premier provides exceptional accuracy at lower applied loads and ensures repeatability. Additionally, it has the potential for high-speed indentation, modulus mapping, and comprehensive scratch testing. These state-of-the-art systems allow us to provide comprehensive mechanical characterization, supporting innovations in materials science, engineering, and biomedical research.