Overview of some prototype specifics

So far melting cut/shredded pieces (>500g) of PP,PE in the oven @ 250C at least 40minutes (not including preheating, folding) then pressing in between heat-resistant fabric and mold gives base tile.


Cut/shredded PP,PE (<500g) can be placed under heat press @240-250C for heating and folding between heat-resistant fabric (only), to be transferred to a mold(with fabric in between) and press.